Figure 4. Effect of the annealed at 100°C during 2 hours on the Optical transmission spectrum in the wavelength range of 200-900 nm for Mo-doped ZnO films prepared at 300°C during 60 minutes

From

Structural and Optical Properties and Relaxation Process of Pulsed Laser Grown and Annealed Mo-doped ZnO Nanostructures

M. Bachir Gaye, C. B. Ndao, E. H. O. Gueye, NM Ndiaye, I Ngom, BD Ngom, B. Lo, P. D. Tall, AC Beye

Physics and Materials Chemistry. 2016, 4(1), 1-5 doi:10.12691/pmc-4-1-1