(a) the quenched alloy in the initial state; (b) A-0; (c) A-2; (d) C-2; (e) B-2 after aging at 140ºС for 1 hour; (f) B-2 after aging at 200ºС for 3 hours. ED patterns showing evolution of the alloy structure after SPD
From
Effect of Severe Plastic Deformation on Structure and Properties of Al-Mg-Si Alloy of 6060 Type
M. Bournane, A. Berezina, О. Davydenko, T. Monastyrska, O. Molebny, V. Spuskanyuk, A. Kotko
Materials Science and Metallurgy Engineering
.
2013
, 1(2), 13-21 doi:10.12691/msme-1-2-1