Figure 2. A plot of Hc/ versus the concentration of PSS, PSE, and SSG polymers (R2 for PSS = 0.9496, for PSE R2= 0.9951, and for SSG R2 = 0.9970)

From

Model Drug Release from Potato Starch-Starch Glycolate Microparticles and Films with and without Incorporated Nano-SiO2

Fateh Eltaboni, Amira Alhodeary, Mona Ibrahim, Fawzia Ali, Aya Al Abdali, Nadin Al Farsi, Fatma Elshibani, Mohamed Ali Sharkasi

Journal of Polymer and Biopolymer Physics Chemistry. 2020, 8(1), 15-27 doi:10.12691/jpbpc-8-1-2