Figure 1. TiO2 film on FTO glass annealed at 1¡ãC/min obtained at (a) 16, (b) 100 and (c) 260X magnifications

From

Effect of Annealing Rates on Surface Roughness of TiO2 Thin films

Benjamin M. John, Simon W. Mugo, James M. Ngaruiya