Figure 1. XRD patterns characteristic of VO2 thin films deposited on soda-lime glass substrate and cooled down to room temperature at a rate of 50°C/min at different oxygen pressures

From

Growth of a-axis Textured Pulsed Laser Deposited VO2 Nanostructures on Glass Substrate

M Thiam, BD Ngom, O Sakho, NM Ndiaye, M Chaker, N Manyala, AC Beye

American Journal of Nanomaterials. 2018, 6(1), 24-33 doi:10.12691/ajn-6-1-3