Figure 1. Microstructure [Magnification: 200X] of as-cast in-situ composite with (a) no Mg; (b)1.5 mass% Mg; (c) 2.5 mass% Mg; (d) 3.5 mass% Mg; (e) 4.0 mass% Mg

From

Effect of Mg on the Wear Behaviour of as-cast Al-4.5Cu-3.4Fe in-situ Composite

Mohammad Sharear kabir, Tamzid Ibn Minhaj, Md Delower Hossain, ASW Kurny

American Journal of Materials Engineering and Technology. 2015, 3(1), 7-12 doi:10.12691/materials-3-1-2