Figure 4. Representative stereomicroscope photomicrographs (magnification x20). A: Depicting failure of GC 1mm sample in veneer itself. B: Depicting mixed failure of GC 2mm sample. C: Depicting adhesive failure of RelyX 1mm sample at the interface of veneer and resin composite, and D: Depicting adhesive failure of Rely X 2mm sample at the interface of veneer and resin composite.

From

Influence of Ceramic Thickness and Luting Agent on the Survival of Bonded Ceramic Veneers. An in-Vitro Study

Alhanoof Aldegheishem, Sara Aljohani, Toleen Moawiah, Shaza Bishti