Table 1. Mean microshear bond strength of Group I and II samples at 24 hours and 7 days

From

Effect of Addition of Novel Chlorhexidine Nanoparticles to a Type II GIC on Its Microshear Bond Strength to Dentin

Tanvi Satpute, Sanjyot Mulay

International Journal of Dental Sciences and Research. 2015, 3(4), 102-106 doi:10.12691/ijdsr-3-4-5