Figure 9. Integrated H2 volume generated by the powdered mixtures preparedat different ZrO2 loadings and optimized sonication time of 60 min at water-splitting and regeneration temperature of 900°C and 1100°C

From

Sonication Derived Powdered Mixtures of Ferrite and Ceramic Nanoparticles for H2 Generation

Vinod S. Amar, Xavier M. Pasala, Jan A. Puszynski, Rajesh V. Shende

American Journal of Energy Research. 2015, 3(2), 25-31 doi:10.12691/ajer-3-2-2