Figure 7. Integrated H2volume generated by NiFe2O4 and NiFe2O4/ZrO2 powdered mixture prepared at different sonication times at water-splitting and regeneration temperatures of 900°C and 1100°C, respectively

From

Sonication Derived Powdered Mixtures of Ferrite and Ceramic Nanoparticles for H2 Generation

Vinod S. Amar, Xavier M. Pasala, Jan A. Puszynski, Rajesh V. Shende

American Journal of Energy Research. 2015, 3(2), 25-31 doi:10.12691/ajer-3-2-2